I have managed to acquire enough slow setting araldite to make up 2 litres (don’t ask) I have made a test batch and it does not seem to give off much if any heat , presumably because it takes 24 hours to set?, will this be suitable to fill the front A post pockets and roughly how much will they hold? or to put it another way will a litre in each be enough?
Cheers On Apr 23, 8:39 am, jin <[email protected]> wrote: > hi all, I need to do the modification to the front inner wing panel to > stop my footwalls filling with water when I wash the car, ive looked > for potting compound but cant find any at a reasonable cost, I have > found this stuff though > > http://cgi.ebay.co.uk/1Kg-General-Casting-Resin-Hardener-Syringe-/230... > > fibreglass casting resin, will it be safe to pour into the cavity > below the front door hinges or will it react / swell / crack the grip > from the inside? > I think ive heard that putting too much resin onto fibreglass causes > it to heat up and warp but im not sure if this is the same stuff? > > Any help much appreciated -- You received this message because you are subscribed to the Google Groups "Quantum Owners Group" group. To post to this group, send email to [email protected] To unsubscribe from this group, send email to [email protected] For more options, visit this group at http://groups.google.com/group/quantumowners?hl=en IMPORTANT NOTE: All information presented herewith is provided on an "As Is" basis, without warranty or the implication thereof. Neither the Quantum Owners Club nor the individuals associated with the Quantum Owners Club or in the preparation of the above information shall have any liability to any person or entity with respect to liability, loss, or damage caused or alleged to be caused directly or indirectly by the instructions contained within this or related message(s).