Dear Yaroslav (and others), Use cylindrical symmetry for flat plate Bragg-Brentano samples. There isn't sufficient information in a single scan to do more than that. Conseqently wnen you used mmm ample symmetry you got "nonsense" (J=400!!). Use POLFPLOT option "A" to plot the resulting "axial distributions" (doesn't work for MArch-Dollase). Bob Von Dreele
R.B. Von Dreele IPNS Division Argonne National Laboratory Argonne, IL 60439-4814 -----Original Message----- From: Yaroslav Mudryk [mailto:[EMAIL PROTECTED] Sent: Friday, February 18, 2005 10:11 AM To: [email protected] Hi everyone, I tried to use spherical harmonics incorporated in EXPGUI/GSAS for modelling a preferential orientation in my sample. I used a cylindrical sample symmetry and it worked fine but I am confused about using such type of symmetry for a flat sample (Bragg-Brentano goniometer). The rolling (mmm) symmetry gave me a texture parameter about 400, which I can not accept. I would appreciate any comments related to this topic. One more question: Does GSAS or any other software have any option for visualization of March-Dollase multi-axis preferential orientation? sorry for using your time, Yaroslav Yaroslav Mudryk 252 Spedding Hall Ames Laboratory Ames, IA 50011, USA Phone: 1-(515)-233-2041