Dear Leonid,

On Sun, 20 Feb 2005 06:20:54 -0800 (PST), Leonid Solovyov wrote:

>
>In this case the problem might be not in the DDM method, but in its
>particular realization in BGMN. The most probable reason is the minimal
>convolution intervals used. For noisy data the interval choice is
>essential.
>
thank you for your discussion. I have set up level 3.5.3, which
uses variable intervals depending from the counting statistics.
We are still testing 3.5.3. If it behaves fine I will set it
online in the next days.

Regards

Joerg Bergmann
*** This EComStation system uptime is 2 days 17 hours ***

Reply via email to