One can also spike the distilled water with previously made CS to increase its initial conductivity. Or go from a batch process to a flow through. For instance my flow through system produces 2 gallons per hour.

Marshall

On 10/13/2014 10:03 AM, Ode Coyote wrote:


The only way to make EIS faster is to use bigger electrodes to spread the current out....or more voltage, but that tends to overload the Nernst Diffusion layer resulting in high silver hydroxide and silver oxide content [ yellow-brown-black CS].

Ode