Ask ENEA they claiml to have found the key cristallographic parameter the
decide if an electrod is nearly always working, just often, or quite never :
*http://www.lenr-canr.org/acrobat/ViolanteVevolutiona.pdf*
*
*
*
*


2013/5/14 DJ Cravens <[email protected]>

> yes the silver alloy (anywhere from 20 to 25 % seems OK with 23% perhaps
> better).  It doesn't seem to load as high but it doesn't "crack" near as
> much.   Regular Pd will often crack as it gets very hard on loading.  My
> personal preference is 5% Rh but the cost is prohibitive.  The 10% Y is
> also good.  The pure Pd (better than 4 nines) is very very temperamental.
>
> ...
>