In message <[email protected]>, dated Tue, 15 Jan 2008, "James, Chris" <[email protected]> writes:
>Coloured anodising is often much harder and is not suitable where >reliable galvanic contact is required. > It's a thicker oxide layer, usually, to get a more uniform colour. -- OOO - Own Opinions Only. Try www.jmwa.demon.co.uk and www.isce.org.uk For very important information, please turn over. John Woodgate, J M Woodgate and Associates, Rayleigh, Essex UK - This message is from the IEEE Product Safety Engineering Society emc-pstc discussion list. Website: http://www.ieee-pses.org/ To post a message to the list, send your e-mail to [email protected] Instructions: http://listserv.ieee.org/request/user-guide.html List rules: http://www.ieee-pses.org/listrules.html For help, send mail to the list administrators: Scott Douglas [email protected] Mike Cantwell [email protected] For policy questions, send mail to: Jim Bacher: [email protected] David Heald: [email protected] All emc-pstc postings are archived and searchable on the web at: http://www.ieeecommunities.org/emc-pstc