Hi Bob,

I have found that hot water leads to a stronger Tyndal beam and greater
colour in CS of equivalent concentration. And unlike Ken (hi Ken) have
found that using seeding  leads to much larger particles. Must be doing
something wrong!

Ivan.

----- Original Message -----
From: "Robert L. Berger" <[email protected]>
To: "Silver-list" <[email protected]>
Sent: Sunday, 19 November 2000 14:13
Subject: CS>development work


> Hi Ya'all,
>
> Is there anyone on this list that has done any kind of study that
> compares any given protocol to make CS when the water temperature is
> varied???
>
> I would appreciate any data or observations that you may have. It
might
> just be the change in T.E. with temperaure.
>
> I want to improve the HVAC ARC CO2 method to get faster "knowdown" of
> pathogens when doing culture studies.
>
> "Ole Bob"
>



--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>